Pacific Northwest National Laboratory has demonstrated a way to turn aluminum-alloy powder directly into rods while removing several preparation steps used in conventional extrusion. In its June 18, 2019 announcement, the laboratory described eliminating canning, vacuum degassing, hot pressing, preheating and removal of the can afterward. [S1]
The conventional route starts by putting loose alloy powder in a can and using a vacuum to remove gases. The can is sealed, hot pressed and heated before entering the extrusion press; afterward, it is stripped away from the consolidated metal. PNNL instead poured Al-12.4TM powder into an open container and pressed a rotating die into it. Heat generated where the die meets the powder softens the material so it can be extruded. The change joins consolidation and shaping instead of preparing a sealed package for the press. [S1]
Called Shear Assisted Processing and Extrusion, or ShAPE, the method still depends on heat. PNNL’s March 2019 explanation says friction heats the contact region and spiral grooves on the die guide softened material toward the extrusion opening. The earlier patent describes applying rotational shear and axial force together: spinning and pushing, rather than pushing alone. The heat is generated at the working interface instead of supplied through a separate preheating step. [S3][S4]
PNNL reported that the powder-derived extrusions stretched two to three times as far before breaking as conventional extrusion products, while retaining equivalent strength. That is a ductility comparison for the reported material, not a finding that every aluminum alloy will behave the same way. The laboratory linked the improvement to changes in small strengthening particles within the aluminum: microscopy showed that ShAPE refined and spread them through the metal. [S1]
The business case remained less settled than the process change. Project leader Scott Whalen said removing steps and preheating could reduce production time, cost and embedded energy. The June announcement supplied no measured cost per finished rod or factory energy saving. For a manufacturer considering a trial, a useful comparison would count the preparation operations avoided alongside the energy used by the extrusion equipment, and then check that the resulting rods meet the required properties. That is a proposed accounting approach, not a saving demonstrated by the announcement. [S1][S3][S4]
SCM Metal Products, a division of Kymera International, supplied the alloy powder and performed mechanical testing. As of the June announcement, it and PNNL were collaborating on a Department of Energy Office of Technology Transitions project to make larger-diameter extrusions. [S1]
Source documents
- A New Manufacturing Process for Aluminum Alloyshttps://www.pnnl.gov/news-media/new-manufacturing-process-aluminum-alloys
- In Great ShAPE™https://www.pnnl.gov/news-media/great-shapetm
- US10189063B2 — System and process for formation of extrusion productshttps://patents.google.com/patent/US10189063B2/en